Almost all seamless steel tubes require straightening at some point in their production process, regardless of the production process, such as drawing, extrusion, hot rolling, or any other process.
The most efficient and productive way to straighten seamless steel pipe is to use an oblique roll straightenerAn oblique roll straightener is one that sets its rollers at an Angle so that the steel tube can be rotated through the straightener
The common method of all types of straighteners is to apply a stress to each part of the steel tube that is higher than the yield point of the seamless steel tube being straightened and then gradually eliminate this stress.
When the seamless steel tube passes through the straightener, it rotates so that each part of the tube can be pressed by the rollers. To ensure this effect, the spacing of each pair of rollers should be designed to allow for lap joints in the width of the pressure applied to the tube.


Galaxy Company Hot Sale Seamless Steel Pipe Products:
seamless steel pipe, line pipe, ASTM A106 pipe, , Mechanical pipe, API 5L pipe, boiler tube,ASTM A335 alloy pipes,GB/T5310 boiler Tube
0users like this.