The heat treatment method of fine grain for steel tube is mainly to heat and cool the steel quickly, so as to achieve a heat treatment process that inhibits the growth of nuclei.

The main methods include cyclic heating quenching refinement and deformation heat treatment refinement technology.


1, Circulating heating quenching Cyclic heating quenching refinement technology refers to the selection of rapid heating can form the minimum temperature of austenite and the shortest heat preservation time for repeated heating and quenching to refine the grain method. The specific process is to heat the steel from room temperature to a slightly higher temperature than AC3 (conventional quenching temperature lower limit), at this temperature for a short period of time insulation for austenite, and then quickly quenched cooling to room temperature, and then repeat this process.


Because of the tendency of recrystallization austenite grain refinement and rapid heating to convert ferrite grains into multiple austenitic grains, the grain is significantly refined, and 1 times per cycle, austenite grains are refined to a certain extent, so as to obtain small austenitic grain tissue.


The results show that when the cyclic quenching is 2-3 times, the austenite grain can be refined to more than 12 grade, the general circulation 3-4 times the best refinement effect, when the cycle 6-7 times, its refinement degree is the greatest. The key of cyclic heating quenching and refining grain technology is heating and cooling speed, which requires fast heating and cooling speed.


If it is not possible to achieve acute heat and acute cooling, can not significantly refine the grain, grain can only reach 10μm, and the production cycle is long, the operation is not convenient, in the actual process production is more restricted.


2. Deformation Heat Treatment


Deformation heat treatment is also an effective heat treatment method to refine grain, which can be divided into high temperature deformation heat treatment and low temperature deformation heat treatment according to the different deformation temperature. High temperature deformation heat treatment is to heat the steel to a slightly higher than AC3 temperature to maintain a period of time to achieve complete austenite, and then at this temperature with a large amount of deformation to make austenite strong deformation, and insulation for a period of time to make austenite initial recrystallization, can be controlled by controlling the high temperature deformation parameters to obtain the required deformation after the phase change austenite


and quenching and tempering before the deformed austenite grains have begun to grow, thus obtaining small martensite tissue. Low temperature deformation heat treatment is the quenching of the steel to the phase change point below the temperature of large pressure deformation, and then heated to AC3 above the temperature for short time insulation, austenite after rapid quenching and tempering.


The results show that the austenitic grains with a size of 0.91μm can be obtained by using the tempering martensite after 80% compression deformation of the low and medium carbon steel, and a very small martensite tissue can be obtained after quenching. Other refined grain heat treatment methods also include multiple rapid heating cooling, circulating heating of the positive fire, etc., but relatively minor. Among the two main methods, the cyclic heating quenching period is too long and the application difficulty is higher than that of deformation heat treatment. In order to achieve the same degree of fine crystal size, deformation heat treatment is easier, and therefore also appears to be more important.