The main performance requirements of oil and gas pipelines include:

(1)Strength

Generally, the oil and gas pipelines are designed according to the yield strength of steel. The use of steel pipe with high yield strength can improve the working pressure of pipeline and obtain better economic benefits: therefore. The yield strength of pipeline steel has been gradually developed from the initial carbon steel, the 1940s) X42 a X52 steel grade. In the late 60 reached X60 a x70 steel grade.
Now the formal production and formal use of yield strength has reached a higher X80~X100 steel grade.

(2) Toughness

In the the 1950s and 60, the rupture of oil and gas pipelines occurred in many parts of the world, through the analysis of these accidents, greatly promoted people's understanding of pipeline toughness indicators. API 5L stipulates that in addition to conventional mechanical performance testing, the production plant should also be in accordance with SR5 and SR6 supplementary requirements of the V-shaped notch summer ratio impact test and drop hammer tearing experiment (that is, DWTT), steel pipe factory should be carried out strict nondestructive testing. Nevertheless, for long-distance pipelines, it is difficult to completely avoid rupture, and it is also necessary to focus on the prevention of crack instability and expansion. The research shows that the control DWTT can be used to achieve the stop cracking.
To this end, many countries around the world have established a minimum value for the percentage of port Shear area of the DWTT test for pipeline steel.

(3) Solderability

Due to the harsh field conditions of the field laying pipeline, steel pipe docking welding requirements have a good solderability. The steel pipe with poor solderability is easy to produce cracks in the weld seam when welding, and causes the hardness of weld and heat affected area to increase, the toughness decreases, and increases the possibility of pipe rupture. The design principle of steel solderability is the control of martensite transition point and quenching rigidity. According to the influence of alloy elements on martensite transition point and the calculation formula of carbon equivalent determined by practical experience, it can be used to evaluate the solderability of steel.
The commonly used formula for carbon equivalence is:
Ceq=w (C) +w (Mn)/6+[w (Cr) +w (Mo) +w (V)]/5 + (W (Ni) +w (Cu))/15 Ceq should generally be controlled at 0. 40% or less. In fact, most steel mills are controlled at 0.
35% or less:

(4) Ductility

 If the ductility is insufficient, it will cause the steel plate to split during the cold bending forming process or to produce a layered tear during the welding process. Therefore, the API standard for pipe welded pipe In addition to the provisions of the flattening test, but also requires a guide bending test.
The key to improving ductility is to reduce the non-metallic inclusions in steel and control the morphology and distribution of inclusions.

 (5) The corrosion resistance

In the transport of sulfur-containing oil and gas, the inner wall of the pipeline contact with hydrogen sulfide and carbon dioxide, resulting in hydrogen embrittlement and stress corrosion rupture. In general, measures such as reducing the sulfur content of steel, controlling sulphide morphology and improving the toughness along the wall thickness direction are generally adopted. Its main feature is through micro-alloying and controlled rolling, in the hot rolling state to obtain high strength, high plasticity, high toughness and good solderability. In order to fully meet the performance requirements of oil and gas pipelines for steel, in addition to strict alloy design, the control of sulfur, phosphorus and other harmful elements is also very strict. The general sulfur content is controlled at 0. 10% below to improve the plasticity and toughness of steel, especially lateral toughness.