The quality problems caused by steel pipe heat treatment are mainly embodied in several aspects (performance, organization, defect, size, surface, etc.).
1 Performance and organizational problems

Performance and organizational problems, depending on the composition and original state of the material and the rationality of the heat treatment process and the level of process control, which is the core of heat treatment quality control content.
The heat treatment process is not well formulated or implemented, the performance of the pipe (such as yield, tensile, extending) will exceed the requirements set by the standard, the organization will appear in the Wei body, ribbon and other standards do not allow the existence of the organization.


2 Dimensions problem

The problem is mainly manifested in the bending of the length direction (axial) and the ellipticity of the cross section direction (radial) and the aberration of the outer diameter.
2.1 Reasons for bending of steel pipe

2.1.1 steel pipe heating uneven production of bending steel pipe heating uneven, along the axial direction of the pipe temperature is different, quenching time is different, the volume of steel pipe change time is different, resulting in bending. 

2.1.2 steel pipe quenching is the preferred heat treatment method for high strength casing and steel pipeline pipe production. The tissue transition is very rapid during quenching, and the tissue transformation of steel pipe brings about volume change.

Bending occurs because the cooling speed of each part of the steel pipe is inconsistent and the speed of the tissue transition is not consistent.

3 Defects and surface problems

3.1 The quenching heating temperature of the quenching crack steel pipe of steel pipe is too high, or the heating time is too long, or the heating temperature is seriously uneven and easy to cause quenching cracks.
If the chemical composition of steel pipe is segregation, steel pipe inclusions are also easy to cause quenching cracks.
3.2 Steel pipe overheating or over-burning steel pipe quenching heating temperature is too high or too long heating time, easy to cause overheating or over burning, serious, steel pipe will collapse.

3.3 When the surface decarbonization or severe oxidation pipe of steel pipe is heated, the surface is seriously decarbonization or seriously oxidized, which is caused by improper control of heating temperature and heating time or adjustment of air-fuel ratio.