There are two methods of expanding pipe with longitudinal rolling and inclined rolling expanding pipe. The quality defects of the longitudinal pipe expanding tube include the cracks of the pipe surface, the uneven wall thickness, the inner straights, the inner pits, the crease and the bending. 

The quality defects of the inclined-rolled pipe-expanding tube are basically the same as those of the two-roll pipe mill, including uneven wall thickness, surface cracks and abrasions, rolling, spiral and spiral inner folds, inner hemp pits and so on. The deformation process of longitudinal tube expansion pipe is drawn and pushed-up type tube expanding process. The deformation process is divided into three stages: under the action of the head cone, the tube wall of the billet tube is deformed first, and with the increasing of the diameter of the head, the diameter of the tube is enlarged and the wall is reduced, and the diameter of the abandoned pipe after the enlarged diameter is determined by the head cylinder. Obviously, the expansion of the diameter is mainly in the second stage. 

The main product defects in longitudinal rolling process are: crack on the surface of waste pipe and crack of tube body, uneven wall thickness, inner straight, crease, inner hemp pit, bending, etc. The pipe-expanding process originated from two perforation process. It is a inclined rolling pipe machine with two conical rolls and horizontally arranged. The diameter of the roll increases gradually from the entrance to the exit of the deformation zone. The roller axis and the rolling line are spatially crossed to form the feeding angle and the rolling angle. Two rollers are single support, respectively driven by 2 motors, the transmission mechanism is located at the outlet side of the pipe rolling machine. The position of the roll can be adjusted along the rolling line axis. The guide plate is arranged up and down. 

The deformation zone is divided into three parts: flattening reducing area, reducing area and turning circle area. Flattening and reducing deformation: the billet pipe is first contacted by the conical roll with cantilever beam state, and advances under the action of friction force. At this time, the billet pipe only contact with the roller, not contact with the head. The deformation is mainly compressed and reduced diameter deformation. The tube wall sometimes thickens when the reduction is too large. 

The size of the flattening reduction zone is related to the position of the head, and the position adjustment of the head is mainly to realize the good mechanical and kinematic conditions for the two bites and the reduction of the diameter and expansion of the blank tube. Reducing wall expansion deformation: it is the main deformation area of inclined rolling expanding pipe. In this area, the billet pipe is reduced wall and enlarged diameter. Since the elongation factor is close to 1, according to the Law of metal volume invariable, the thin metal of the tube wall becomes the metal which needs to be supplemented by the increase of outer diameter. The deformation of metal mainly occurs in the circumferential and radial of the billet tube. As the rollers and the head can be moved along the respective axis, so long as the roll and the position of the head can be changed, the expansion of the size of the waste pipe. 

When the position of the roll and the head is adjusted, the deformation amount of the wall area is not changed. Rotary deformation: The billet tube after the reduction of wall expansion deformation, no longer contact with the head and into the circle area. 

Under the action of the surface friction, the waste pipe is smoothly separated from the deformation zone. The extension factor of the inclined-rolling pipe-expanding process is 1. In the case of the main deformation, some superfluous additional deformations inevitably occur. The additional deformation of the metal will result in the defect of the waste pipe and increase the energy consumption of the rolling. The additional deformation of metal includes additional torsional deformation, additional axial shearing deformation and additional circumferential shearing deformation. The reason of the additional deformation, the deformation process and the two-roll taper roll piercing machine with feeding angle and rolling angle, and the process of rolling pipe mill are basically the same. However, due to the inclined rolling expansion tube, the cone angle of the expansion head is relatively large, and the use of fixed guide plate instead of the active guide, the length of the roll is also relatively short. Therefore, three kinds of additional deformation caused by inclined-rolling expansion tube are different in the distribution and size of deformation and the process of two-roll inclined-rolling machine and pipe-rolling machine, that is, the additional torsion deformation is smaller, the additional axial shearing is larger. The inclined rolling expansion tube is similar to the two-roll extension machine in structure, and the expansion process and deformation characteristics are same as that of the two-roll inclined pipe mill. The difference between the two is: the latter hope that the billet tube in the case of deformation, deformation of metal is mainly an axial extension, and control the amount of spread, the former requires the billet tube in the deformation, deformation of the metal should mainly occur transverse spread and control its axial extension, elongation coefficient of 1, or even less than 1, That is, the tube diameter of the billet is enlarged but the length is constant or shortened. 

Therefore, the cone angle of the expander head will be very large, and the rolling angle and feeding angle are also relatively large. The defects of the pipe-expanding tube are: uneven wall thickness, surface cracks and abrasions, rolling, spiral and spiral inner fold, inner hemp pits, etc. Because the diameter of the inclined rolling pipe is large, the probability of crack on the surface of the pipe is higher. In addition, the spiral channel of the surface is more serious when the pipe is inclined to spread. For this purpose, the proper length of the roller and the corresponding wall area can be considered when designing the hole. In the mean wall area, the normal distance between the head surface and the roll surface is equal. At the same time, the proper reduction of the diameter is also conducive to the improvement of wall thickness accuracy. Although the roller shape design and adjustment to reduce the pipe wall thickness uneven and surface spiral road, but after all, the skew rolling expansion tube deformation is very large and the roll length is also short. There are still different degrees of uneven wall thickness and spiral path in the waste pipe expanded by inclined rolling. 

For this reason, the wall thickness accuracy of the waste pipe can be improved obviously after the inclined rolling and expanding process. Generally speaking, when the pipe is inclined to spread, the billet tube will oxidize in the inner and outer surface during the heating process. The iron oxide peel of the billet tube can be removed by high pressure water in front of the head to improve the inner surface quality and the life of the head.