steel pipe
The Introduction Of Precision Tube
Precision tube is a kind of ordinary seamless steel tube (or ERW welded steel tube) through the process of fine drawing or cold rolling. Due to the precision bright tube inside and outside wall no oxide layer, under high pressure no leakage, high precision, high finish, cold bending no deformation, flaming, flattening no cracks and other points, so mainly used to produce pneumatic or hydraulic components of the product, such as cylinder or cylinder, can be seamless, but also welded pipe.
The chemical components of precision bright tube are C, Si, Mn, S, P, Cr. High quality carbon steel, finishing rolling, no oxidation bright heat treatment (NBK state), non-destructive testing, the inner wall of the steel tube with special equipment scrubbing and through high pressure washing, anti-rust oil on the steel tube for anti-rust treatment, both ends of the sealing for dust treatment. The inner and outer wall of the steel tube is of high precision and high finish. After heat treatment, the steel tube has no oxidation layer and the inner wall is of high cleanness. The steel tube bears high pressure, does not deform during cold bending, expands and flattens without cracks. Steel tube color: white with bright, with a higher metallic luster.
Main application:
Automobile, mechanical parts and other steel pipe project.
Steel grade Silicon carbide manganese phosphorus sulfur
10# 0.07~0.13 0.17~0.37 0.35~0.65 ≤0.035 ≤0.035
20# 0.17~0.23 0.17~0.37 0.35~0.65 ≤0.035 ≤0.035
35# 0.32~0.39 0.17~0.37 0.35~0.65 ≤0.035 ≤0.035
45# 0.42~0.50 0.17~0.37 0.50~0.80 ≤0.035 ≤0.035
40cr 0.37~0.44 0.17~0.37 0.50~0.80 ≤0.035 ≤0.035
25Mn 0.22~0.2 0.17~0.37 0.70~1.00 ≤0.035 ≤0.035
37Mn5 0.30~0.39 0.15~0.30 1.20~1.50 ≤0.015 ≤0.020

0users like this.