The Main Factors For Decarbonization Of Steel Pipes
When the steel pipe is heated, on the basis of the iron oxide, the carbon atoms in the surface layer of the unoxidized steel pipe diffuse outwards, the oxygen atoms in the furnace gas also diffuse inwards through the iron oxide skin, when the two diffusions meet, the carbon atoms are burned, resulting in the lack of carbon of the unoxided steel surface layer.This phenomenon is called decarbonization.
Carbon is one of the main elements that determine the properties of steel, decarbonization makes steel hardness, wear resistance, fatigue strength, impact toughness, service life and other mechanical properties significantly reduced. It is very harmful to the tool steel, ball bearing steel, spring steel, high carbon steel and so on, and even due to decarbonization exceeds the regulations result in waste, so decarbonization is one of the key problems in steel production. The main factors affecting decarbonization are heating temperature, heating time, atmosphere in the furnace, in addition to the chemical composition of steel also has a certain effect on decarbonization.
1, The effect of heating temperature on decarbonization:
The effect of heating temperature on the thickness of the visible decarbonization layer of the billet varies depending on the steel, generally with the heating temperature increases, it can be seen that the thickness of the decarbonization layer increased significantly.
2, The effect of heating time on decarbonization, the longer the heating time, the larger the thickness of the decarbonized layer, so, shorten the heating time, especially shorten the billet with high temperature after the stay time in the furnace. Rapid heating is an effective measure to reduce the decarbonization of the billet
3, The atmosphere in the furnace on the decarbonization: The atmosphere in the furnace on decarbonization is fundamental, the atmosphere in the furnace H2O, H2, O2, and CO2 can cause decarbonization, while CO and CH4 can increase steel carbon.
4, The chemical composition of steel on decarbonization effect:
The higher the carbon content of steel, heating more easily decarbonized, if the steel contains aluminum, tungsten, cobalt and other elements, then decarbonization increased. If the steel contains chromium, manganese, boron and other elements, then decarbonization reduction.