steel pipe
The Three Main Methods Of Identifying Welded Steel Pipes And Seamless Steel Pipes:
Metallographic analysis. The method is one of the main methods to distinguish welded steel pipe and seamless steel pipe. High-frequency resistance welding steel pipe does not add welding material, if the use of rough grinding and re-corrosion method can not clearly see the weld. However, the completion of high-frequency resistance welding steel pipe welding will result in the difference between the weld tissue and the steel pipe mother material. Welded steel pipes and seamless steel pipes can be distinguished by the metallographic method.
In the process of identifying the two types of steel pipes, it is necessary to cut samples of length and width of 40mm at the welding site, to rough grinding, fine grinding and polishing, and then placed under the microscope to observe the tissue, then master material and weld area tissue can be accurately identified.
2. Corrosion method. In the process of using corrosion method to identify welded steel pipe and seamless steel pipe, should be soldered at the welding steel pipe weld, after grinding should be able to see the traces of polishing, and then in the weld with sandpaper grinding the end face, and with 5% of the nitric acid alcohol solution to treat the end face, if there is a clear weld, It can be proved that the steel pipe is a welded steel pipe.There is no significant difference in the end surface of the seamless steel pipe after corrosion.3. Microidentification: Micro-identification with metallographic microscope, adjust the light path and magnification of the microscope, starting from the lower multiple, the whole cross-section of observation, found that welding signs are difficult to confirm, using a higher multiple for further analysis and confirmation. Depending on the existence of welding tissue characteristics, the identification is clear whether the welded steel pipe or seamless steel pipe.

0users like this.