The first mode of production:
Welded into pipe by direct molding of steel plate, belt, the main process of which is strip forming, welding and setting diameter.
Features: Less production process, simple engineering process, short production cycle, slightly lower product accuracy.
The second mode of production: By the steel plate, belt first directly formed welded to a certain size pipe, and then through cold drawing or cold rolling into the finished pipe, commonly known as DOM welded steel pipe.
Its main processes are forming, welding, fixed diameter, cold rolling or cold drawing (with mandrel or no core rod), or continuous cold drawing (that is, welding-cold drawing joint production line).
Features: Dispersion of production processes, long process and production cycle, large footprint, good product size accuracy, smooth internal and external surface, mechanical properties and good metallographic tissue status.
The third mode of production: By the steel plate, belt first directly formed and welded into a certain size pipe, into a continuous diameter reducer for cold reduction into the finished pipe.
Its main process is forming, welding, continuous cold reduction diameter.
Features: Compact production process, simple process flow, high production efficiency of the Unit, specifications range transformation fast, suitable for the production of small diameter and thin-walled welded steel pipe.

 