The causes and solutions of cold drawing honing pipe concave folding phenomenon

The causes and solutions of cold drawing honing pipe concave folding phenomenon

First, cold drawing honing pipe concave folding disadvantages

With the transparency and openness of the market, the user's requirements for the cylinder are becoming higher and higher, so the requirements for the cold-drawn honing pipe as the user of the cylinder manufacturing are also becoming higher and higher.

The use of poor quality cold drawn honing pipes will have the following effects:

Short service life of hydraulic cylinder;

The cylinder is prone to oil leakage;

The clearance of piston rod, guide sleeve and cylinder is not easy to match;

Influence the accumulation of long-term partners.


Second, the reasons for this situation may be:

Due to the empty drawing thin-walled pipe, the diameter reduction is too large or the transition of the steel pipe hammer head is too urgent.

Raw material steel pipe situation is too thin.

The honing equipment is too old.


Third, cold drawing honing pipe concave folding phenomenon our specific treatment method:

It is necessary for the manufacturer to allocate the reducing amount reasonably;

Check the hammer head to confirm whether the hammer head is smooth and wrinkle-free;

Check that the length and width of the grinding position of the pipe material must be appropriate;

Timely maintenance and replacement of product equipment are equally. important.



 

Galaxy Company Steel Pipe Product Hot Tags:

OCTG, casing, seamless steel pipe, line pipe, boiler tube, ASTM A333 pipe, API 5L pipe,, welded steel pipe, steel pipe inventory,  Chinese pipe factory, API 5L X52 pipe, pipe fittings, tubing, API 5CT pipe, Steel pipe

 

You Might Also Like

  • I'm interested in your products, please contact me.
  • I want to know the details of your products.
  • I want to know the specific price of your products.
  • I want to know the specific information of your company.
  • Whether your company can provide product samples.
  • Please inform the minimum price of this batch of goods.
  • Please inform the minimum number of batches of the product.
  • Please inform the payment methods of cooperation, logistics methods, etc.
  • How long does it take for delivery?
  • How much is shipping?
Send